We know that the enamel reactor has excellent properties such as corrosion resistance, and in order to make it to play its advantages, it is necessary to carry out correct operation to prevent the equipment from being damaged due to improper operation, and can not play its advantages, mixing is an important part of this process. Let's take a look at how to do it.
1, drop, heat preservation process to often check the temperature of enamel reactor, pressure, a comprehensive look at the drop of materials, materials in the reactor, and do the corresponding records. When the temperature and pressure of the reactor and the interface of the material are abnormal, the corresponding measures should be taken in time to adhere to the normal reaction form in order to prevent the occurrence of equipment and personal accidents.
2, take the reactor material to stop stirring for more than 2 minutes, to ensure that no other safety risks can be stopped. Do not use easy to fall, hard metal container out of the reactor sampling, so as not to scratch enamel surface.
3. After putting the material into the reactor, the relevant valve should be adjusted to a suitable open-close position, and the agitation can be opened, if the reactor is found to have distinct music and vibration and other abnormal need emergency stop disposal. If the reactor is mixed with solid powder, etc. , need to be fully dissolved before you can start stirring.
4. The circulating water of the relevant condenser should be opened before the electric heating of the reactor. Should first turn over drain bypass valve, slowly turn over the steam valve, drain water, pipe bypass valve, a trap to stop the drain task, so that the jacket preheating.
The above is the correct operation of the agitation of the enamel reactor, and for the equipment, not only this step, but all the operations should be carried out according to the regulations, so as to avoid the occurrence of accidents, make the equipment last longer.